各国Inconel625标准大全:合金 板材 价格
中英对照说明:
Rod:杆 Bar:棒 Wire:线材 Forging Stock:锻件
Plate:中厚板 Sheet:薄板 Strip:钢带
Pipe:管 Tube:细管
Rings:环件 Welded Tube:无缝管 Seamless Pipe:焊管
---------------------------------------------------------------
棒材:
ASTM B 446; ASME SB 446 (Rod & Bar),
AMS 5666 (Bar, Forgings, & Rings);
ISO 9723 (Rod & Bar),
VdTüV 499 (Rod & Bar),
BS 3076NA21 (Rod & Bar),
EN 10095 (Rod, Bar, & Sections),
DIN 17752 (Rod & Bar),
ASME Code Case 1935 (Rod, Bar, & Forgings),
线材:
DIN 17753 (Wire).
ISO 9724 (Wire)
AMS 5837 (Wire),
锻件:
ISO 9725 (Forgings),
ASTM B 564; ASME SB 564 (Forgings);
DIN 17754 (forgings),
板材:
ASTM B 443; ASTM SB 443 (Plate, Sheet & Strip),
AMS 5599; 5869; MAM 5599 (Plate, Sheet & Strip),
ISO 6208 (Plate, Sheet & Strip),
VdTüV 499 (Plate, Sheet & Strip),
BS 3072NA21 (Plate & Sheet),
EN 10095 (Plate, Sheet & Strip),
DIN 17750 (Plate, Sheet & Strip),
ASME Code Case 1935.
管材:
ASTM B 444; ASTM B 829;
ASME SB444; ASME SB 829 (Seamless Pipe & Tube),
ASTM B704; ASTM B 751; ASME SB 704;
ASME SB 751 (Welded Tube),
ASTM B705; ASTM B 775; ASME SB 705;
ASME SB 775 (Welded Pipe),
ISO 6207 (Tube),
AMS 5581 (Seamless & Welded Tube),
VdTüV 499 (Tube),
BS 3074NA21 (Seamless Pipe & Tube),
DIN 17751 (Tube),
ASME Code Case 1935.
----------------------------------------------------------
在民用工业的很多领域,服役的构件材料都处于高温的腐蚀环境中。为满足市场需要,根据材料的使用环境,归类出系列Inconel625 。
1、Inconel625 母合金系列
2、抗腐蚀Inconel625 板、棒、丝、带、管及锻件
3、高强度、耐腐蚀Inconel625 棒材、弹簧丝、焊丝、板、带材、锻件
4、耐玻璃腐蚀系列产品
5、环境耐蚀、硬表面耐磨Inconel625 系列
6、特种精密铸造零件(叶片、增压涡轮、涡轮转子、导向器、仪表接头)
7、玻棉生产用离心器、高温轴及辅件8、钢坯加热炉用钴基合金耐热垫块和滑轨
9、阀门座圈
10、铸造“U”形电阻带
11、离心铸管系列
12、纳米材料系列产品
13、轻比重高温结构材料
14、功能材料(膨胀合金、高温高弹性合金、恒弹性合金系列)
15、生物医学材料系列产品
16、电子工程用靶材系列产品
17、动力装置喷嘴系列产品
18、司太立合金耐磨片
19、超高温抗氧化腐蚀炉辊、辐射管。
●更多信息
请直接与我公司服务人员联络(热线电话:021-67768089),
以获得更多的有关Inconel625耐蚀合金新技术参数数据以及其它 inconel|英科奈尔系列的选择、应用、热处理及库存等相关资料。