Power plant flue gas desulphurization and denitration equipment is supplied with thermal power station equipment, which can effectively control air pollution. Coal-fired thermal power equipment at work, it will produce chloride containing a large amount of environmental pollution. In the chloride ion concentration exceeds 10,000ppm environment, the use of flue gas desulphurization equipment 6Mo super corrosion resistant stainless steel and high nickel alloys (eg Hastelloy) designed to reduce air pollution control, reduce equipment corrosion loss and prolong life. Common desulfurization and denitrification have special materials: 254SMO, AL-6XN, Cronifer 1925hMo (1.4529), INCONEL 690, Hastelloy HASTELLOY C-276, HASTELLOY C-22 ...