Depending on the environment, medical titanium and titanium alloys selected are not the same. If you need a good ductility, optionally titanium (Gr.1-Gr.4); If you need good strength after heat treatment should be selected 1300Mpa strength of titanium alloy. Characters memory alloy titanium base is also important class of titanium products in the medical field applications.